In this work, the silylation of sodium montmorillonite (Na-MMT) was performed in glycerol using 3-aminopropyltriethoxysilane, N-(2-aminoethyl)-3-aminopropyltrimethoxysilane and 3-[2-(2-aminoethylamino) ethylamino]-propyl-trimethoxysilane. The effects on the d-spacing of sodium montmorillonite (Na- MMT) upon reaction with three aminosilanes of different chain length were studied in details by combining experimental and computational techniques. Infrared spectroscopy was used to monitor the grafting process, while the degree of grafting was calculated using thermogravimetric analysis. X-ray diffraction experiments were carried out to evaluate the shift of the (0 0 1) basal spacing. It was found that the degree of silylation of Na-MMT increases with increasing the length of the aminosilane organic moieties, the overall aminosilane concentration, and temperature. The same beneficial effects were observed on the silicate d-spacing, as its value increases with increasing silane concentration and reaction temperature. Remarkably, however, increasing the length of the organic chains in the silane modifiers resulted in decreasing values of the Na-MMT interlayer distance. A rationale for this behavior is proposed on the basis of atomistic molecular dynamics simulation evidences.
Sodium montmorillonite silylation: Unexpected effect of the aminosilane chain length / F., Piscitelli; P., Posocco; R., Toth; M., Fermeglia; S., Pricl; Mensitieri, Giuseppe; M., Lavorgna. - In: JOURNAL OF COLLOID AND INTERFACE SCIENCE. - ISSN 0021-9797. - STAMPA. - 351:(2010), pp. 108-115. [10.1016/j.jcis.2010.07.059]
Sodium montmorillonite silylation: Unexpected effect of the aminosilane chain length
MENSITIERI, GIUSEPPE;
2010
Abstract
In this work, the silylation of sodium montmorillonite (Na-MMT) was performed in glycerol using 3-aminopropyltriethoxysilane, N-(2-aminoethyl)-3-aminopropyltrimethoxysilane and 3-[2-(2-aminoethylamino) ethylamino]-propyl-trimethoxysilane. The effects on the d-spacing of sodium montmorillonite (Na- MMT) upon reaction with three aminosilanes of different chain length were studied in details by combining experimental and computational techniques. Infrared spectroscopy was used to monitor the grafting process, while the degree of grafting was calculated using thermogravimetric analysis. X-ray diffraction experiments were carried out to evaluate the shift of the (0 0 1) basal spacing. It was found that the degree of silylation of Na-MMT increases with increasing the length of the aminosilane organic moieties, the overall aminosilane concentration, and temperature. The same beneficial effects were observed on the silicate d-spacing, as its value increases with increasing silane concentration and reaction temperature. Remarkably, however, increasing the length of the organic chains in the silane modifiers resulted in decreasing values of the Na-MMT interlayer distance. A rationale for this behavior is proposed on the basis of atomistic molecular dynamics simulation evidences.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.